Pronounced seams

How can I improve the seams on my parts? Pressure advance is tuned for good square corners right now. Rapido HF, 0.6mm CHT nozzle, PLA. 0.3mm layer height.
No description
3 Replies
sherbs
sherbs2y ago
Start experimenting with wipe & retraction settings... You can improve on it a bit from where it is
absent-sapphire
absent-sapphire2y ago
Same problem with petg, did you solved?
beejayf
beejayf2y ago
Could be the pressure advance settings.