Retraction calibration help

After changing my hot end, I started running a reaction tower, changing retraction length by 0.01mm per layer starting from 0 and going all the way to 2.65mm nothing seems to have changed. PetG, 230c, retract speed 60mm/s. I haven't yet tuned for PA
No description
5 Replies
sherbs
sherbs15mo ago
Have you tuned other settings? That brim looks a little suspect... Makes me wonder what a test cube looks like... Maybe something going on that is more fundamental than retraction issue?
MACBEAN
MACBEAN15mo ago
No description
No description
No description
No description
No description
MACBEAN
MACBEAN15mo ago
Y- 20.13 X- 20.25 Z- 20.10
rival-black
rival-black15mo ago
Is this the same roll of filament you used immediately prior to changing the nozzle? Same gcode for the calibration cube as before nozzle change? Assuming nothing else has changed, I’d guess this filament needs drying.
MACBEAN
MACBEAN15mo ago
Best invest in a filament dryer then and see what difference that makes