PETG defect on same place of print

Hi, when printing PETG I keep getting this defect in the same spot. With part cooling set to 10% it appears, and with 40% it’s still present but slightly less noticeable. Do you have any advice? Using OrcaSlicer 2.2.
No description
No description
No description
4 Replies
Torque
Torque2mo ago
Post some more pics of the slicer paths. That pic you have up there only shows travel
Jarda
JardaOP2mo ago
slicer paths? not understand..
Jarda
JardaOP2mo ago
Zits always appear where travel, first screenshot with Avoid crossing walls enabled in OrcaSlicer. Less Zits.
No description
No description
Yathani
Yathani4w ago
Temp might be high for this PETG. Run temp tower and choose best one. If you are using rapido, i read that temp reading is lower than actual